Typical Properties |
|
Heat Treat State |
Typical |
Density (lb/cu.in. @ 68F)
|
|
.101
|
Electrical Conductivity (% IACS @ 68F)
|
|
27
|
Thermal Conductivity (cal/sec/sq cm/cm/C @ 25C)
|
|
0.26
|
Coefficient of Thermal Expansion (per F @ 68-212F)
|
|
11.9
|
Coefficient of Thermal Expansion (per F @ 68-572F)
|
|
12.7
|
Melting Range (Liquidus-Solidus)(F)
|
|
960-1120
|
Resistance to Hot Cracking
|
|
VG
|
Pressure Tightness
|
|
VG
|
Fluidity
|
|
VG
|
Solidification Shrinkage Tendency
|
|
VG
|
Strength at Elevated Temperatures
|
|
G
|
Corrosion Resistance
|
|
G
|
Machinability
|
|
G
|
Polishing
|
|
F
|
Gas Welding
|
|
VG
|
Arc Welding
|
|
VG
|
Brazing
|
|
No
|
Normally Heat Treated
|
|
Optional
|
Annodizing Appearance
|
|
Gray
|
Electroplating
|
|
VG
|
Compressive Yield Strength (ksi)
|
F
|
19
|
Hardness (Brinell) (HB @ 500kg)
|
F
|
70
|
Shear Strength (ksi)
|
F
|
22
|
Endurance Limit (K ksi)
|
F
|
10
|
Compressive Yield Strength (ksi)
|
T5
|
27
|
Hardness (Brinell) (HB @ 500kg)
|
T5
|
80
|
Shear Strength (ksi)
|
T5
|
24
|
Endurance Limit (K ksi)
|
T5
|
11
|
Compressive Yield Strength (ksi)
|
T6
|
25
|
Hardness (Brinell) (HB @ 500kg)
|
T6
|
80
|
Shear Strength (ksi)
|
T6
|
29
|
Endurance Limit (K ksi)
|
T6
|
11
|