Typical Properties |
|
Heat Treat State |
Typical |
Compressive Yield Strength (ksi)
|
|
25
|
Hardness (Brinell) (HB @ 500kg)
|
|
75
|
Shear Strength (ksi)
|
|
26
|
Endurance Limit (K ksi)
|
|
9
|
Modulus of Elasticity (K ksi)
|
|
9.7
|
Density (lb/cu.in. @ 68F)
|
|
.100
|
Electrical Conductivity (% IACS @ 68F)
|
|
30
|
Thermal Conductivity (cal/sec/sq cm/cm/C @ 25C)
|
|
0.29
|
Coefficient of Thermal Expansion (per F @ 68-212F)
|
|
13.4
|
Coefficient of Thermal Expansion (per F @ 68-572F)
|
|
14.6
|
Melting Range (Liquidus-Solidus)(F)
|
|
1100-1180
|
Resistance to Hot Cracking
|
|
F
|
Pressure Tightness
|
|
F
|
Fluidity
|
|
G
|
Solidification Shrinkage Tendency
|
|
F
|
Strength at Elevated Temperatures
|
|
F
|
Corrosion Resistance
|
|
E
|
Machinability
|
|
E
|
Polishing
|
|
E
|
Gas Welding
|
|
F
|
Arc Welding
|
|
G
|
Brazing
|
|
Yes
|
Normally Heat Treated
|
|
No
|
Annodizing Appearance
|
|
Light Yellow
|