Typical Properties |
|
Heat Treat State |
Typical |
Modulus of Elasticity (ksi)
|
|
18000
|
Machinability (% of free cutting brass)
|
|
10
|
Fatigue Strength (10^8 cycles) (ksi)
|
|
13
|
Impact Strength (Charpy) (ft-lb)
|
|
100
|
Compressive Strength (0.100 in. set/in.) (ksi)
|
|
37
|
Melting Range (Liquidus-Solidus)(F)
|
|
2010-2100
|
Coefficient of Thermal Expansion (per F @ 68-400F)
|
|
0.0000095
|
Thermal Conductivity (Btu/sq.ft/ft./hr/F @ 68F)
|
|
26
|
Specific Heat (Btu/lb/F @ 68F)
|
|
0.09
|
Electrical Conductivity (% IACS @ 68F)
|
|
11
|
Density (lb/cu.in. @ 68F)
|
|
0.323
|
Patternmakers Shrinkage (in/ft)
|
|
3/16
|
Drossing
|
|
Low
|
Gassing
|
|
High
|
Fluidity
|
|
High
|
Shrinkage
|
|
High
|
Casting Yield
|
|
Low
|